EN 12163 Grade CuNi2Si solution heat-treated, cold worked, precipitation hardened and cold worked

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

10 %

Show Material materials with Elongation of 10 %

Elongation A100

20.0 °C

6 %

Show Material materials with Elongation A100 of 6 %

Hardness, Vickers

20.0 °C

190 - 250 [-]

Show Material materials with Hardness, Vickers of 190 - 250 [-]

Tensile strength

20.0 °C

640 - 700 MPa

Show Material materials with Tensile strength of 640 - 700 MPa

Yield strength Rp0.2

20.0 °C

620 - 680 MPa

Show Material materials with Yield strength Rp0.2 of 620 - 680 MPa

Thermal

PropertyTemperatureValue

Specific heat capacity

20.0 °C

377 J/(kg·K)

Show Material materials with Specific heat capacity of 377 J/(kg·K)

Chemical properties

PropertyValue

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Nickel

1.6 - 2.5 %

Show Material materials with Nickel of 1.6 - 2.5 %

Silicon

0.4 - 0.8 %

Show Material materials with Silicon of 0.4 - 0.8 %