Material CuAl7Si2 (CW302G) is incomparable to a DIN-make. It is used in the form of bars, profiles, prematerial for forged parts and forged parts.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.7 g/cm³

Show Material materials with Density of 7.7 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 - 130 GPa

Show Material materials with Elastic modulus of 110 - 130 GPa

Typical for Leaded Phosphor Bronze

Elongation

20.0 °C

12 %

Show Material materials with Elongation of 12 %

Elongation A10

20.0 °C

10 %

Show Material materials with Elongation A10 of 10 %

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Leaded Phosphor Bronze

Tensile strength

20.0 °C

600 MPa

Show Material materials with Tensile strength of 600 MPa

Yield strength Rp0.2

20.0 °C

350 MPa

Show Material materials with Yield strength Rp0.2 of 350 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.5E-5 - 1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K

Typical for Leaded Phosphor Bronze

Specific heat capacity

23.0 °C

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K)

Typical for Leaded Phosphor Bronze

Chemical properties

PropertyValue

Aluminium

6.3 - 7.6 %

Show Material materials with Aluminium of 6.3 - 7.6 %

Copper

88.55 %

Show Material materials with Copper of 88.55 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Manganese

0.2 %

Show Material materials with Manganese of 0.2 %

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

Silicon

1.5 - 2.2 %

Show Material materials with Silicon of 1.5 - 2.2 %

Tin

0.2 %

Show Material materials with Tin of 0.2 %

Zinc

0.5 %

Show Material materials with Zinc of 0.5 %