EN 12163 Grade CuAl10Ni5Fe4 R740

Want to keep this datasheet? Save it now in your required format

Description

CuAl10Ni5Fe4 (CW307G) is a wrought alloy of high strength, also at increased temperatures. The strength properties of cold formable wrought alloys are primarily dependent on the deformation grade. Tensile strength, yield strength and hardness rise according to the increasing cold forming grade. Elongation after fracture and contraction at fracture are decreasing. Thermal conductivity is reduced by the Al-content, electrical conductivity decreases according to the increasing AL-content. CuAl10Ni5Fe4 has a high strength at high temperatures up to approx. 300°C and a high endurance strength also at corrosion strain. The alloy is particularly resistant to cavitation , shows a high wear resistance, and a high corrosion resistance to saltwater, sulfite bases and mineral acids. Processing properties: warm forming: good cold forming: unfavorable machinability: moderately soft soldering: unfavorable hard soldering: moderately gas-shielded welding: very good burnishing: good The material is used for plates for condenser and heat transfer bottoms, for shafts, screws, wear parts as well as for controlling parts for hydraulic appliances, hot steam instruments, high voltage switchers, suction rolls in paper industry, cylinder corebushings for combustion engines, mechanically and chemically loaded parts in machine and shipbuilding and mining.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.6 g/cm³

Show Material materials with Density of 7.6 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

120 GPa

Show Material materials with Elastic modulus of 120 GPa

Elongation

20.0 °C

8 %

Show Material materials with Elongation of 8 %

Elongation A11.3

20.0 °C

6 %

Show Material materials with Elongation A11.3 of 6 %

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Leaded Phosphor Bronze

Shear modulus

20.0 °C

45 GPa

Show Material materials with Shear modulus of 45 GPa

Tensile strength

20.0 °C

740 MPa

Show Material materials with Tensile strength of 740 MPa

Yield strength Rp0.2

20.0 °C

400 - 530 MPa

Show Material materials with Yield strength Rp0.2 of 400 - 530 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.5E-5 - 1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K

Typical for Leaded Phosphor Bronze

Specific heat capacity

20.0 °C

420 J/(kg·K)

Show Material materials with Specific heat capacity of 420 J/(kg·K)

Thermal conductivity

20.0 °C

50 - 57 W/(m·K)

Show Material materials with Thermal conductivity of 50 - 57 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

4.00E+6 - 7.00E+6 S/m

Show Material materials with Electrical conductivity of 4.00E+6 - 7.00E+6 S/m

Specific Electrical conductivity

10.3 % IACS

Show Material materials with Specific Electrical conductivity of 10.3 % IACS

Chemical properties

PropertyValue

Aluminium

8.5 - 11 %

Show Material materials with Aluminium of 8.5 - 11 %

Copper

76.05 %

Show Material materials with Copper of 76.05 %

Iron

3 - 5 %

Show Material materials with Iron of 3 - 5 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

4 - 6 %

Show Material materials with Nickel of 4 - 6 %

Silicon

0.2 %

Show Material materials with Silicon of 0.2 %

Tin

0.1 %

Show Material materials with Tin of 0.1 %

Zinc

0.4 %