EN 12168 Grade CuZn36Pb2As H070

Want to keep this datasheet? Save it now in your required format

Description

CW602N is suited for cold forming, easy to machine and resistant to dezincification. Application: water supply

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.4 - 8.46 g/cm³

Show Material materials with Density of 8.4 - 8.46 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

105 GPa

Show Material materials with Elastic modulus of 105 GPa

Elongation

20.0 °C

25 %

Show Material materials with Elongation of 25 %

Hardness, Brinell

20.0 °C

70 - 150 [-]

Show Material materials with Hardness, Brinell of 70 - 150 [-]

Hardness, Vickers

20.0 °C

75 - 130 [-]

Show Material materials with Hardness, Vickers of 75 - 130 [-]

Shear modulus

23.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Typical for Wrought Copper Brass

Tensile strength

20.0 °C

280 - 350 MPa

Show Material materials with Tensile strength of 280 - 350 MPa

Yield strength Rp0.2

20.0 °C

100 - 150 MPa

Show Material materials with Yield strength Rp0.2 of 100 - 150 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-5 - 2.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K

Typical for Wrought Copper Brass

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

20.0 °C

377 J/(kg·K)

Show Material materials with Specific heat capacity of 377 J/(kg·K)

Thermal conductivity

20.0 °C

110 - 114 W/(m·K)

Show Material materials with Thermal conductivity of 110 - 114 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

1.47E+7 S/m

Show Material materials with Electrical conductivity of 1.47E+7 S/m

Specific Electrical conductivity

25 % IACS

Show Material materials with Specific Electrical conductivity of 25 % IACS

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Arsenic

0.02 - 0.15 %

Show Material materials with Arsenic of 0.02 - 0.15 %

Copper

61 - 63 %

Show Material materials with Copper of 61 - 63 %

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

1.7 - 2.8 %

Show Material materials with Lead of 1.7 - 2.8 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Tin

0.1 %

Show Material materials with Tin of 0.1 %