363 Molybdenum Stress Relieved

Want to keep this datasheet? Save it now in your required format

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

10 g/cm³

Show Material materials with Density of 10 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Elastic modulus

330 GPa

Show Material materials with Elastic modulus of 330 GPa at 23.0 °C

23.0 °C

Elongation

6.3 %

Show Material materials with Elongation of 6.3 % at 23.0 °C

23.0 °C

Poisson's ratio

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-] at 23.0 °C

23.0 °C

Typical for Molybdenum

Shear modulus

125 GPa

Show Material materials with Shear modulus of 125 GPa at 23.0 °C

23.0 °C

Typical for Molybdenum

Tensile strength

730 MPa

Show Material materials with Tensile strength of 730 MPa at 23.0 °C

23.0 °C

Yield strength

630 MPa

Show Material materials with Yield strength of 630 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperatureComment

Coefficient of thermal expansion

2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2E-5 1/K at 23.0 °C

23.0 °C

Melting point

2610 °C

Show Material materials with Melting point of 2610 °C

Typical for Molybdenum

Specific heat capacity

250 J/(kg·K)

Show Material materials with Specific heat capacity of 250 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

117 - 431 W/(m·K)

Show Material materials with Thermal conductivity of 117 - 431 W/(m·K) at 23.0 °C

23.0 °C

Typical for Molybdenum

Chemical properties

Property

Carbon

0.01 - 0.03 %

Iron

0 - 0.01 %

Molybdenum

99.3 - 99.5 %

Nickel

0 - 2E-3 %

Nitrogen

0 - 2E-3 %

Oxygen

0 - 3E-3 %

Silicon

0 - 0.01 %

Titanium

0.4 - 0.55 %

Zirconium

0.06 - 0.12 %