See where UNS R05200 Cold Worked falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ17 g/cm³ at 23 °C
Coefficient of thermal expansion
α6.5E-6 1/K at 23 °C
Melting point
Tm2996 °C
Typical for Tantalum
Specific heat capacity
cp140 J/(kg·K) at 23 °C
Thermal conductivity
λ52 - 57 W/(m·K) at 23 °C
Typical for Tantalum
Element
Weight %
Comment
99.8 - 100 %
0 - 0.01 %
0 - 1.5E-3 %
0 - 0.01 %
0 - 0.02 %
This material data has been provided by MakeItFrom.com.