Murdotec® 1000 traffic red

Alternative and trade names
Murdotec 1000 traffic red, UHMWPE, UHMW-PE
Want to keep this datasheet? Save it now in your required format

Description

Murdotec® 1000 coloured, our UHMW-PE, is ideally suited for use where good wear and abrasion resistance along with excellent slide properties are required. This material also has excellent machining properties.

With a molecular weight of around 5 million g/mol, this plastic always meets top quality requirements and is also approved by the EU and FDA.

This material is quickly available in lots of RAL colours.


Some of the key characteristics are:

  • Good anti-adhesion properties
  • Good resistance to chemicals
  • Very high shock and impact absorption
  • Good machinability
  • Electrically isolating

    sheet group 1.2

    Opertaing conditions: Rough operation

    Available in Sheet and Rod form

  • Related Standards

    This material data has been provided by Murdotec Kunststoffe GmbH & Co. KG.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Coefficient of friction

    0.2 [-]

    Show Supplier Material materials with Coefficient of friction of 0.2 [-]

    Coefficient of friction, kinetic

    0.2 [-]

    Show Supplier Material materials with Coefficient of friction, kinetic of 0.2 [-]

    against steel (0.25m/s, 0.25N/mm)

    Density

    23.0 °C

    0.94 g/cm³

    Show Supplier Material materials with Density of 0.94 g/cm³

    max., DIN 53479, ISO 1183

    Moisture absorption

    23.0 °C

    0 %

    Show Supplier Material materials with Moisture absorption of 0 %

    no moisture absorption

    Molar mass

    5.00E+6 g/mol

    Show Supplier Material materials with Molar mass of 5.00E+6 g/mol

    Water absorption

    23.0 °C

    0.01 %

    Show Supplier Material materials with Water absorption of 0.01 %

    Water absorption, saturation

    23.0 °C

    0.01 %

    Show Supplier Material materials with Water absorption, saturation of 0.01 %

    max., DIN 53715, till 96h

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    0.7 GPa

    Show Supplier Material materials with Elastic modulus of 0.7 GPa

    min., DIN 53457, ISO 527-2

    Elongation

    23.0 °C

    300 %

    Show Supplier Material materials with Elongation of 300 %

    min., DIN 53455, ISO 527-2

    Hardness, Ball Indentation

    23.0 °C

    30 MPa

    Show Supplier Material materials with Hardness, Ball Indentation of 30 MPa

    min., DIN 53456, ISO 2039

    Hardness, Shore D

    23.0 °C

    61 - 65 [-]

    Show Supplier Material materials with Hardness, Shore D of 61 - 65 [-]

    DIN 868, ISO 7619-1

    Impact strength, Charpy notched

    23.0 °C

    170 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 170 kJ/m²

    min., DIN 53453, ISO 179

    Yield strength

    23.0 °C

    20 MPa

    Show Supplier Material materials with Yield strength of 20 MPa

    DIN 53455, ISO 527-2

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    2E-4 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 2E-4 1/K

    Heat deflection temperature

    42 °C

    Show Supplier Material materials with Heat deflection temperature of 42 °C

    Heat deflection temperature, 1.80 MPa

    42 °C

    Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 42 °C

    ISO 75-A

    Max service temperature

    80 - 90 °C

    Show Supplier Material materials with Max service temperature of 80 - 90 °C

    Max service temperature, continuous

    80 °C

    Show Supplier Material materials with Max service temperature, continuous of 80 °C

    DIN 53446, in air for 20000h

    Max service temperature, short

    90 °C

    Show Supplier Material materials with Max service temperature, short of 90 °C

    in air

    Melting point

    130 - 135 °C

    Show Supplier Material materials with Melting point of 130 - 135 °C

    ISO 3146 method C

    Min service temperature

    -200 °C

    Show Supplier Material materials with Min service temperature of -200 °C

    Thermal conductivity

    23.0 °C

    0.4 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.4 W/(m·K)

    DIN 52612

    Flammability

    UL94: HB, for 3/6mm

    Electrical

    PropertyTemperatureValueComment

    Comparative tracking index

    23.0 °C

    600 V

    Show Supplier Material materials with Comparative tracking index of 600 V

    Dielectric strength

    23.0 °C

    45 kV/mm

    Show Supplier Material materials with Dielectric strength of 45 kV/mm

    max., DIN 53481, ISO 60243

    Surface resistivity

    23.0 °C

    1.00E+12 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1.00E+12 Ω/sq

    min., DIN 53482, ISO 60093

    Volume resistivity

    23.0 °C

    1.00E+12 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1.00E+12 Ω·cm

    min., DIN 53482, ISO 60093

    Technological properties

    Property
    Application areas

    Wear-resistant bearings, profiles and segments, chain guides


    Conveyor: Conveyor elements, Conveyor troughs, Conveyor slide lining, Conveyors stars, Antistatic sliding elements, Curved tracks, Curve guides, Conveyor belts


    Sliding: Sliding rails, Sliding profiles, Sliding segments


    Other applications: Wiping strips, Feed hooper, Outlets, Belt stripping, Bins, Gaskets, Format sets, Guiding elements, Sliding elements, Plain bearing, Link belts, Highly wear-resistant sliding elements, Chain guides, Sprockets, Crane support plates, Bearing bushes, Baffle plates, Moulding stripes, Pump parts, Belt guides, Rolls, Chain-pulled conveyors, Control discs, Transport chutes, Deflections pulleys, Wear bars, Workpiece carriers, Toothed wheels, Centrifuges

    Certifications

    Food Contact EU:Yes, FDA:Yes

    Color

    Traffic Red

    Wear resistance

    Sand Slurry Test: 100% ISO 15527