General
Property | Temperature | Value | Comment |
---|---|---|---|
Adhesion | 23.0 °C | 93 N Show Supplier Material materials with Adhesion of 93 N | min., Hot U Test |
Linear density | 23.0 °C | 3.76E-3 - 4.24E-3 g/cm Show Supplier Material materials with Linear density of 3.76E-3 - 4.24E-3 g/cm |
Dimension
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Nominal breaking force | 23.0 °C | 258 N Show Supplier Material materials with Nominal breaking force of 258 N | Tensile Member: E Glass |
Technological properties
Property | ||
---|---|---|
Color | Brown | |
Cord Construction | 330.1/0 | |
Other | Manufacturing Location: Canada | |
Processing history | Latex Type: Chloroprene, Dip Pick-Up: 17 to 23% | |
Twist per Meter | 52 - 68 TPM | Direction: S & Z |
Do you have a technical question or need more information about this material?
Post it as a comment below and receive answers from engineers and other community members.