Glass cord A10-060402

Alternative and trade names
Glass Cord
Want to keep this datasheet? Save it now in your required format

Description

SBR latex impregnated E glass cord (Elastomer Polymer Matrix Composite)

This material data has been provided by NGF Glass.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Adhesion

23.0 °C

93 N

Show Supplier Material materials with Adhesion of 93 N

min., Hot U Test

Linear density

23.0 °C

3.76E-3 - 4.24E-3 g/cm

Show Supplier Material materials with Linear density of 3.76E-3 - 4.24E-3 g/cm

Dimension

PropertyValue

Bobbin Inner Diameter

60 mm

Show Supplier Material materials with Bobbin Inner Diameter of 60 mm

Bobbin Length

356 mm

Show Supplier Material materials with Bobbin Length of 356 mm

Flange Diameter

190.5 mm

Show Supplier Material materials with Flange Diameter of 190.5 mm

Mechanical

PropertyTemperatureValueComment

Nominal breaking force

23.0 °C

258 N

Show Supplier Material materials with Nominal breaking force of 258 N

Tensile Member: E Glass

Technological properties

Property
Color

Brown

Cord Construction

330.1/0

Other

Manufacturing Location: Canada

Processing history

Latex Type: SBR, Dip Pick-Up: 17 to 23%

Twist per Meter

52 - 68 TPM