Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.83 g/cm³

Show Supplier Material materials with Density of 7.83 g/cm³

Dimension

PropertyValue

Inside diameter

400 - 730 mm

Show Supplier Material materials with Inside diameter of 400 - 730 mm

Length

1750 - 3370 mm

Show Supplier Material materials with Length of 1750 - 3370 mm

Outside diameter

450 - 910 mm

Show Supplier Material materials with Outside diameter of 450 - 910 mm

Thickness

150 - 230 mm

Show Supplier Material materials with Thickness of 150 - 230 mm

Width

1350 - 2540 mm

Show Supplier Material materials with Width of 1350 - 2540 mm

Chemical properties

PropertyValue

Arsenic

0 - 0.08 %

Show Supplier Material materials with Arsenic of 0 - 0.08 %

Carbon

0.42 - 0.5 %

Show Supplier Material materials with Carbon of 0.42 - 0.5 %

Chromium

0 - 0.25 %

Show Supplier Material materials with Chromium of 0 - 0.25 %

Copper

0 - 0.25 %

Show Supplier Material materials with Copper of 0 - 0.25 %

Iron

Balance

Manganese

0.5 - 0.8 %

Show Supplier Material materials with Manganese of 0.5 - 0.8 %

Nickel

0 - 0.25 %

Show Supplier Material materials with Nickel of 0 - 0.25 %

Phosphorus

0 - 0.04 %

Show Supplier Material materials with Phosphorus of 0 - 0.04 %

Silicon

0.17 - 0.37 %

Show Supplier Material materials with Silicon of 0.17 - 0.37 %

Sulfur

0 - 0.04 %

Show Supplier Material materials with Sulfur of 0 - 0.04 %

Technological properties

Property
Application areas

Steel forgings are applied for manufacture of the details of machinery and spare parts for metallurgical, mining and machine-building equipment.

Processing methods

Manufactured by open die forging