General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 0.83 - 0.89 g/cm³ Show Supplier Material materials with Density of 0.83 - 0.89 g/cm³ at 23.0 °C | 23.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 1100 % Show Supplier Material materials with Elongation of 1100 % at 23.0 °C | 23.0 °C | min., ASTM D412 (500 mm/min) |
Hardness, Shore A | 5 - 11 [-] Show Supplier Material materials with Hardness, Shore A of 5 - 11 [-] at 23.0 °C | 23.0 °C | ASTM D2240 |
Modulus at 100% elongation | 9.9E-5 GPa Show Supplier Material materials with Modulus at 100% elongation of 9.9E-5 GPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Modulus at 300% elongation | 1.6E-4 GPa Show Supplier Material materials with Modulus at 300% elongation of 1.6E-4 GPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Tear strength | 9.79 kN/m Show Supplier Material materials with Tear strength of 9.79 kN/m at 23.0 °C | 23.0 °C | ASTM D624 Die C (500 mm/min) |
Tensile strength | 2.81 MPa Show Supplier Material materials with Tensile strength of 2.81 MPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Rheological Properties
Property | Value | Temperature | Comment |
---|---|---|---|
Melt mass-flow rate | 21.6 g/10min Show Supplier Material materials with Melt mass-flow rate of 21.6 g/10min | ASTM D1238, 190°C/1.2kg | |
Shrinkage | 1.9 - 2.5 % Show Supplier Material materials with Shrinkage of 1.9 - 2.5 % at 23.0 °C | 23.0 °C | ASTM D955 |
Shrinkage, transverse | 1.7 - 2.3 % Show Supplier Material materials with Shrinkage, transverse of 1.7 - 2.3 % at 23.0 °C | 23.0 °C | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Shoes insole, medical appliances | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3 | |
Color | Transparent | |
Other | Overmolding capabilities: PP |