TPE-S PHOENIX™ 01101

Alternative and trade names
THERMOLAST®, Monprene®, Versaflex™, Dryflex®
Want to keep this datasheet? Save it now in your required format

Description

This grade is an easy processing Thermoplastic Elastomer (TPE) designed for injection molding applications that have FDA requirements. The key features are: Soft touch, easy to process and color, rubber like texture and feel, excellent weather resistance, excellent tensile strength, excellent elasticity, meet FDA requirements

This material data has been provided by Phon Tech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTemperatureComment

Density

0.83 - 0.89 g/cm³

Show Supplier Material materials with Density of 0.83 - 0.89 g/cm³ at 23.0 °C

23.0 °C

ASTM D792

Mechanical

PropertyValueTemperatureComment

Elongation

1100 %

Show Supplier Material materials with Elongation of 1100 % at 23.0 °C

23.0 °C

min., ASTM D412 (500 mm/min)

Hardness, Shore A

7 - 13 [-]

Show Supplier Material materials with Hardness, Shore A of 7 - 13 [-] at 23.0 °C

23.0 °C

ASTM D2240

Modulus at 100% elongation

1.5E-4 GPa

Show Supplier Material materials with Modulus at 100% elongation of 1.5E-4 GPa at 23.0 °C

23.0 °C

ASTM D412 (500 mm/min)

Modulus at 300% elongation

2.3E-4 GPa

Show Supplier Material materials with Modulus at 300% elongation of 2.3E-4 GPa at 23.0 °C

23.0 °C

ASTM D412 (500 mm/min)

Tear strength

8.83 kN/m

Show Supplier Material materials with Tear strength of 8.83 kN/m at 23.0 °C

23.0 °C

ASTM D624 Die C (500 mm/min)

Tensile strength

2.7 MPa

Show Supplier Material materials with Tensile strength of 2.7 MPa at 23.0 °C

23.0 °C

ASTM D412 (500 mm/min)

Rheological Properties

PropertyValueTemperatureComment

Melt mass-flow rate

11.2 g/10min

Show Supplier Material materials with Melt mass-flow rate of 11.2 g/10min

ASTM D1238, 190°C/1.2kg

Shrinkage

2.3 - 2.9 %

Show Supplier Material materials with Shrinkage of 2.3 - 2.9 % at 23.0 °C

23.0 °C

ASTM D955

Shrinkage, transverse

2.2 - 2.8 %

Show Supplier Material materials with Shrinkage, transverse of 2.2 - 2.8 % at 23.0 °C

23.0 °C

ASTM D955

Technological properties

Property
Application areas

Shoes insole, medical appliances, fishing lure, sports equipment, toys

Certifications

REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3

Color

Transparent

Other

Overmolding capabilities: PP