Description

This grade is an easy processing Thermoplastic Elastomer (TPE) designed for injection molding applications that bonds to various materials like PC, ABS, PA, PC/ABS, SAN. The key features are: Excellent bonding to ABS; PC; PC/ABS; PA; SAN, good appearance, rubber like feel, excellent tensile strength, good tear strength

Properties

General

Density ρ

1.19 - 1.25 g/cm³ at 20 °C

ASTM D792

Melt mass-flow rate MFR

90 g/10min at 20 °C

ASTM D1238 (200°C, 5kg)

Shrinkage cshrink

0.6 - 1.2 % at 20 °C

ASTM D955

Shrinkage, transverse cshrink, trans

0.6 - 1.2 % at 20 °C

ASTM D955

Mechanical

Elongation A

578.6 % at 20 °C

ASTM D412 (500 mm/min)

Hardness, Shore A HS A

57 - 63 [-] at 20 °C

ASTM D2240

Modulus at 100% elongation EA=100

2.4452610000000002E-3 GPa at 20 °C

ASTM D412 (500 mm/min)

Modulus at 300% elongation EA=300

3.995510999999999E-3 GPa at 20 °C

ASTM D412 (500 mm/min)

Tear strength Rtear

30.44 kN/m at 20 °C

ASTM D624 Die C (500 mm/min)

Tensile strength Rm

6.61 MPa at 20 °C

ASTM D412 (500 mm/min)

Technological properties

Application areas

Electrical and pneumatic tool grip, electronic appliances, tool grip

Color

Black

Processing methods

Injection molding

This material data has been provided by Phon Tech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.