TPE-S PHOENIX™ 12602

Alternative and trade names
THERMOLAST®, Monprene®, Versaflex™, Dryflex®
Want to keep this datasheet? Save it now in your required format

Description

This grade is an easy processing Thermoplastic Elastomer (TPE) designed for injection molding applications that bonds to various materials like PC, ABS, PA, PC/ABS, SAN. The key features are: Excellent bonding to ABS; PC; PC/ABS; PA; SAN, good appearance, rubber like feel, excellent tensile strength, good tear strength

This material data has been provided by Phon Tech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 - 1.25 g/cm³

Show Supplier Material materials with Density of 1.19 - 1.25 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

577.6 %

Show Supplier Material materials with Elongation of 577.6 %

ASTM D412 (500 mm/min)

Hardness, Shore A

23.0 °C

57 - 63 [-]

Show Supplier Material materials with Hardness, Shore A of 57 - 63 [-]

ASTM D2240

Modulus at 100% elongation

23.0 °C

2.5E-3 GPa

Show Supplier Material materials with Modulus at 100% elongation of 2.5E-3 GPa

ASTM D412 (500 mm/min)

Modulus at 300% elongation

23.0 °C

4.03E-3 GPa

Show Supplier Material materials with Modulus at 300% elongation of 4.03E-3 GPa

ASTM D412 (500 mm/min)

Tear strength

23.0 °C

33.38 kN/m

Show Supplier Material materials with Tear strength of 33.38 kN/m

ASTM D624 Die C (500 mm/min)

Tensile strength

23.0 °C

7.76 MPa

Show Supplier Material materials with Tensile strength of 7.76 MPa

ASTM D412 (500 mm/min)

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

36.9 g/10min

Show Supplier Material materials with Melt mass-flow rate of 36.9 g/10min

ASTM D1238, 200°C/5kg

Shrinkage

23.0 °C

1.3 - 1.9 %

Show Supplier Material materials with Shrinkage of 1.3 - 1.9 %

ASTM D955

Shrinkage, transverse

23.0 °C

1.1 - 1.7 %

Show Supplier Material materials with Shrinkage, transverse of 1.1 - 1.7 %

ASTM D955

Technological properties

Property
Application areas

Electrical and pneumatic tool grip, electronic appliances, tool grip

Certifications

REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3

Color

White

Fillers

Calcium Carbonate

Other

Overmolding capabilities: ABS, AS, PMMA, PA