Property | Value | Testing Standard |
---|---|---|
Density | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Density of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Compression set | 23 °C | 18.5 [-] Show Supplier Material materials with Compression set of 18.5 [-] | ASTM D395 B | |
70 °C | 51.2 [-] Show Supplier Material materials with Compression set of 51.2 [-] | ASTM D395 B | ||
Elongation | 874.7 % Show Supplier Material materials with Elongation of 874.7 % | ASTM D412 | 500 mm/min | |
Hardness, Shore A | 42 - 48 [-] Show Supplier Material materials with Hardness, Shore A of 42 - 48 [-] | ASTM D2240 | ||
Modulus at 100% elongation | 0.00097 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.00097 GPa | ASTM D412 | 500 mm/min | |
Modulus at 300% elongation | 0.0015 GPa Show Supplier Material materials with Modulus at 300% elongation of 0.0015 GPa | ASTM D412 | 500 mm/min | |
Tear strength | 14.6 kN/m Show Supplier Material materials with Tear strength of 14.6 kN/m | ASTM D624 Die C | 500 mm/min | |
Tensile strength | 3.7 MPa Show Supplier Material materials with Tensile strength of 3.7 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 34.2 g/10min Show Supplier Material materials with Melt mass-flow rate of 34.2 g/10min | ASTM D1238 | 190°C/2.16kg |
Shrinkage | 1.4 - 2 % Show Supplier Material materials with Shrinkage of 1.4 - 2 % | ASTM D955 | Transverse |
1.5 - 2.1 % Show Supplier Material materials with Shrinkage of 1.5 - 2.1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliances, tool grip, toothbrush, pen grip | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | Translucent | |
Other | Overmolding capabilities: PP |