TPE-S PHOENIX™ 03452

Alternative and trade names
THERMOLAST®, Monprene®, Versaflex™, Dryflex®
Want to keep this datasheet? Save it now in your required format

Description

This grade is an easy processing Thermoplastic Elastomer (TPE) designed for extrusion and injection molding applications that have FDA requirements. The key features are: Soft touch, excellent scratch endurance, easy to process and color, excellent tensile strength, good elasticity, excellent weather resistance, overmoldable to Polypropylene, meet FDA requirements

This material data has been provided by Phon Tech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.85 - 0.91 g/cm³

Show Supplier Material materials with Density of 0.85 - 0.91 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

744.7 %

Show Supplier Material materials with Elongation of 744.7 %

ASTM D412 (500 mm/min)

Hardness, Shore A

23.0 °C

42 - 48 [-]

Show Supplier Material materials with Hardness, Shore A of 42 - 48 [-]

ASTM D2240

Modulus at 100% elongation

23.0 °C

9E-4 GPa

Show Supplier Material materials with Modulus at 100% elongation of 9E-4 GPa

ASTM D412 (500 mm/min)

Modulus at 300% elongation

23.0 °C

1.7E-3 GPa

Show Supplier Material materials with Modulus at 300% elongation of 1.7E-3 GPa

ASTM D412 (500 mm/min)

Tear strength

23.0 °C

19.18 kN/m

Show Supplier Material materials with Tear strength of 19.18 kN/m

ASTM D624 Die C (500 mm/min)

Tensile strength

23.0 °C

4.39 MPa

Show Supplier Material materials with Tensile strength of 4.39 MPa

ASTM D412 (500 mm/min)

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

13.6 g/10min

Show Supplier Material materials with Melt mass-flow rate of 13.6 g/10min

ASTM D1238, 200°C/5kg

Shrinkage

23.0 °C

1.8 - 2.4 %

Show Supplier Material materials with Shrinkage of 1.8 - 2.4 %

ASTM D955

Shrinkage, transverse

23.0 °C

1.5 - 2.1 %

Show Supplier Material materials with Shrinkage, transverse of 1.5 - 2.1 %

ASTM D955

Technological properties

Property
Application areas

Syringe stopper, seal, gasket, dropper bulb, pen grip, sport equipment

Certifications

REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements

Color

Translucent

Other

Overmolding capabilities: PP