TPE-S PHOENIX™ 03906

Alternative and trade names
THERMOLAST®, Monprene®, Versaflex™, Dryflex®
Want to keep this datasheet? Save it now in your required format

Description

This grade is an easy processing Thermoplastic Elastomer (TPE) designed for injection molding applications. The key features are: Excellent scratch endurance, excellent wear resistance, easy to process and color, excellent tensile strength, good elasticity, excellent weather resistance, good appearance, overmoldable to Polypropylene

This material data has been provided by Phon Tech.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueTemperatureComment

Density

0.85 - 0.91 g/cm³

Show Supplier Material materials with Density of 0.85 - 0.91 g/cm³ at 23.0 °C

23.0 °C

ASTM D792

Mechanical

PropertyValueTemperatureComment

Elongation

815.5 %

Show Supplier Material materials with Elongation of 815.5 % at 23.0 °C

23.0 °C

ASTM D412 (500 mm/min)

Hardness, Shore A

87 - 93 [-]

Show Supplier Material materials with Hardness, Shore A of 87 - 93 [-] at 23.0 °C

23.0 °C

ASTM D2240

Modulus at 100% elongation

5.27E-3 GPa

Show Supplier Material materials with Modulus at 100% elongation of 5.27E-3 GPa at 23.0 °C

23.0 °C

ASTM D412 (500 mm/min)

Modulus at 300% elongation

6.61E-3 GPa

Show Supplier Material materials with Modulus at 300% elongation of 6.61E-3 GPa at 23.0 °C

23.0 °C

ASTM D412 (500 mm/min)

Tear strength

67.79 kN/m

Show Supplier Material materials with Tear strength of 67.79 kN/m at 23.0 °C

23.0 °C

ASTM D624 Die C (500 mm/min)

Tensile strength

18.42 MPa

Show Supplier Material materials with Tensile strength of 18.42 MPa at 23.0 °C

23.0 °C

ASTM D412 (500 mm/min)

Rheological Properties

PropertyValueTemperatureComment

Melt mass-flow rate

2.7 g/10min

Show Supplier Material materials with Melt mass-flow rate of 2.7 g/10min

ASTM D1238, 200°C/5kg

Shrinkage

1.5 - 2.1 %

Show Supplier Material materials with Shrinkage of 1.5 - 2.1 % at 23.0 °C

23.0 °C

ASTM D955

Shrinkage, transverse

1.4 - 2 %

Show Supplier Material materials with Shrinkage, transverse of 1.4 - 2 % at 23.0 °C

23.0 °C

ASTM D955

Technological properties

Property
Application areas

Caster wheel, automotive interior

Certifications

REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3

Color

Translucent

Other

Overmolding capabilities: PP