General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 0.95 - 1.01 g/cm³ Show Supplier Material materials with Density of 0.95 - 1.01 g/cm³ at 23.0 °C | 23.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 927.6 % Show Supplier Material materials with Elongation of 927.6 % at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Hardness, Shore A | 57 - 63 [-] Show Supplier Material materials with Hardness, Shore A of 57 - 63 [-] at 23.0 °C | 23.0 °C | ASTM D2240 |
Modulus at 100% elongation | 1.61E-3 GPa Show Supplier Material materials with Modulus at 100% elongation of 1.61E-3 GPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Modulus at 300% elongation | 2.27E-3 GPa Show Supplier Material materials with Modulus at 300% elongation of 2.27E-3 GPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Tear strength | 23.94 kN/m Show Supplier Material materials with Tear strength of 23.94 kN/m at 23.0 °C | 23.0 °C | ASTM D624 Die C (500 mm/min) |
Tensile strength | 6.15 MPa Show Supplier Material materials with Tensile strength of 6.15 MPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Rheological Properties
Property | Value | Temperature | Comment |
---|---|---|---|
Melt mass-flow rate | 54.3 g/10min Show Supplier Material materials with Melt mass-flow rate of 54.3 g/10min | ASTM D1238, 190°C/5kg | |
Shrinkage | 1.2 - 1.8 % Show Supplier Material materials with Shrinkage of 1.2 - 1.8 % at 23.0 °C | 23.0 °C | ASTM D955 |
Shrinkage, transverse | 1.2 - 1.8 % Show Supplier Material materials with Shrinkage, transverse of 1.2 - 1.8 % at 23.0 °C | 23.0 °C | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Syringe gasket, window seal | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements, Bio-Compatible | |
Color | Black | |
Fillers | Calcium Carbonate | |
Other | Overmolding capabilities: PP |