General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 0.85 - 0.92 g/cm³ Show Supplier Material materials with Density of 0.85 - 0.92 g/cm³ at 23.0 °C | 23.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Compression set | 24.8 [-] Show Supplier Material materials with Compression set of 24.8 [-] at 23.0 °C | 23.0 °C | ASTM D395 B, 22hrs |
68.1 [-] Show Supplier Material materials with Compression set of 68.1 [-] at 70.0 °C | 70.0 °C | ASTM D395 B, 22hrs | |
Elongation | 755.7 % Show Supplier Material materials with Elongation of 755.7 % at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Hardness, Shore A | 67 - 73 [-] Show Supplier Material materials with Hardness, Shore A of 67 - 73 [-] at 23.0 °C | 23.0 °C | ASTM D2240 |
Modulus at 100% elongation | 2.63E-3 GPa Show Supplier Material materials with Modulus at 100% elongation of 2.63E-3 GPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Modulus at 300% elongation | 3.82E-3 GPa Show Supplier Material materials with Modulus at 300% elongation of 3.82E-3 GPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Tear strength | 41.17 kN/m Show Supplier Material materials with Tear strength of 41.17 kN/m at 23.0 °C | 23.0 °C | ASTM D624 Die C (500 mm/min) |
Tensile strength | 7.38 MPa Show Supplier Material materials with Tensile strength of 7.38 MPa at 23.0 °C | 23.0 °C | ASTM D412 (500 mm/min) |
Rheological Properties
Property | Value | Temperature | Comment |
---|---|---|---|
Melt mass-flow rate | 5.9 g/10min Show Supplier Material materials with Melt mass-flow rate of 5.9 g/10min | ASTM D1238, 190°C/5kg | |
Shrinkage | 1.5 - 2.1 % Show Supplier Material materials with Shrinkage of 1.5 - 2.1 % at 23.0 °C | 23.0 °C | ASTM D955 |
Shrinkage, transverse | 1.3 - 1.9 % Show Supplier Material materials with Shrinkage, transverse of 1.3 - 1.9 % at 23.0 °C | 23.0 °C | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Tubes | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements, Bio-Compatible | |
Color | Translucent | |
Other | Overmolding capabilities: PP |