General
Property | Value | Testing Standard |
---|---|---|
Density | 0.85 - 0.91 g/cm³ Show Supplier Material materials with Density of 0.85 - 0.91 g/cm³ | ASTM D792 |
Mechanical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Elongation | 1100.1 % Show Supplier Material materials with Elongation of 1100.1 % | ASTM D412 | 500 mm/min |
Modulus at 100% elongation | 3e-05 GPa Show Supplier Material materials with Modulus at 100% elongation of 3e-05 GPa | ASTM D412 | 500 mm/min |
Modulus at 300% elongation | 5e-05 GPa Show Supplier Material materials with Modulus at 300% elongation of 5e-05 GPa | ASTM D412 | 500 mm/min |
Tear strength | 3.9 kN/m Show Supplier Material materials with Tear strength of 3.9 kN/m | ASTM D624 Die C | 500 mm/min |
Tensile strength | 0.355 MPa Show Supplier Material materials with Tensile strength of 0.355 MPa | ASTM D412 | 500 mm/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 416.7 g/10min Show Supplier Material materials with Melt mass-flow rate of 416.7 g/10min | ASTM D1238 | 150°C/2.16kg |
Shrinkage | 2.2 - 2.8 % Show Supplier Material materials with Shrinkage of 2.2 - 2.8 % | ASTM D955 | Transverse |
3 - 3.6 % Show Supplier Material materials with Shrinkage of 3 - 3.6 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical appliances, rehabilitation ball, sticker, toys and many more | |
Certifications | REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3, Meets FDA requirements | |
Color | Transparent | |
Processing methods |
Do you have a technical question or need more information about this material?