TPE-S PHOENIX™ 10901

Alternative and trade names
THERMOLAST®, Monprene®, Versaflex™, Dryflex®
Want to keep this datasheet? Save it now in your required format

Description

This grade is an easy processing TPE designed for injection molding applications, containing post industrial recycled content, The key features are:

  • Soft touch
  • Overmolded to polypropylene
  • Rubber like texture and feel
  • Easy to process
  • Non toxic

  • This material data has been provided by Phon Tech.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.05 - 1.1 g/cm³

    Show Supplier Material materials with Density of 1.05 - 1.1 g/cm³

    ASTM D792

    Recycled Content

    35 - 45 %

    Show Supplier Material materials with Recycled Content of 35 - 45 %

    Mechanical

    PropertyTemperatureValueComment

    Elongation

    23.0 °C

    397.3 %

    Show Supplier Material materials with Elongation of 397.3 %

    ASTM D412 (500 mm/min)

    Hardness, Shore A

    23.0 °C

    87 - 93 [-]

    Show Supplier Material materials with Hardness, Shore A of 87 - 93 [-]

    ASTM D2240

    Modulus at 100% elongation

    23.0 °C

    5.7E-3 GPa

    Show Supplier Material materials with Modulus at 100% elongation of 5.7E-3 GPa

    ASTM D412 (500 mm/min)

    Modulus at 300% elongation

    23.0 °C

    6.3E-3 GPa

    Show Supplier Material materials with Modulus at 300% elongation of 6.3E-3 GPa

    ASTM D412 (500 mm/min)

    Tear strength

    23.0 °C

    45.32 kN/m

    Show Supplier Material materials with Tear strength of 45.32 kN/m

    ASTM D624 Die C (500 mm/min)

    Tensile strength

    23.0 °C

    6.65 MPa

    Show Supplier Material materials with Tensile strength of 6.65 MPa

    ASTM D412 (500 mm/min)

    Rheological Properties

    PropertyTemperatureValueComment

    Melt mass-flow rate

    17.6 g/10min

    Show Supplier Material materials with Melt mass-flow rate of 17.6 g/10min

    ASTM D1238, 190°C/2.16kg

    Shrinkage

    23.0 °C

    1.5 - 2.1 %

    Show Supplier Material materials with Shrinkage of 1.5 - 2.1 %

    ASTM D955

    Shrinkage, transverse

    23.0 °C

    1.1 - 1.7 %

    Show Supplier Material materials with Shrinkage, transverse of 1.1 - 1.7 %

    ASTM D955

    Technological properties

    Property
    Application areas

    Tool Grip and many more...

    Certifications

    REACH SVHC free, RoHS 2.0, GS AfPS GS 2019:01 PAK, EN 71-3

    Color

    Black

    Processing methods

    Injection Molding
    Nozzle:
    Front:
    Center:
    Rear:
    190℃~185℃
    185℃~180℃
    180℃~175℃
    170℃~165℃