Description

The Graphite-particles show a primary particle size of <100 nm with spherical shape. It consists of pure Carbon with remarkably low Oxygen content <2%.

This material data has been provided by RHI Magnesita GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size

50 - 60 nm

Show Supplier Material materials with Particle size of 50 - 60 nm

max.

Chemical properties

PropertyValue

Carbon

97.82 %

Show Supplier Material materials with Carbon of 97.82 %

Oxygen

1.9 %

Show Supplier Material materials with Oxygen of 1.9 %

Technological properties

Property
Other

Summary of the EDX-analysis for SiC:



Spot 1
ElementWt-%Atom.-%
C93.2897.82
O2.421.9


The EDX-measurements show no signs of impurities besides oxygen. In comparison with other nano-graphite/graphene powders the oxygen content is remarkably low.