General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Density of 1.27 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 20 GPa Show Supplier Material materials with Elastic modulus of 20 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 1 % Show Supplier Material materials with Elongation of 1 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 18.1 GPa Show Supplier Material materials with Flexural modulus of 18.1 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 179 MPa Show Supplier Material materials with Flexural strength of 179 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 42 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 42 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 42 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 42 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 106 MPa Show Supplier Material materials with Tensile strength of 106 MPa | ASTM D 638 | break |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Monitoring and Imaging | |
Availability | Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |