LEXAN™ Copolymer FXE1414T - Americas

Want to keep this datasheet? Save it now in your required format

Description

Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.19 g/cm³

Show Supplier Material materials with Density of 1.19 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.09 %

Show Supplier Material materials with Moisture absorption of 0.09 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.19 [-]

Show Supplier Material materials with Relative density of 1.19 [-]

ASTM D 792 |

Water absorption

23.0 °C

0.13 %

Show Supplier Material materials with Water absorption of 0.13 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.3 GPa

Show Supplier Material materials with Elastic modulus of 2.3 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

5.4 %

Show Supplier Material materials with Elongation of 5.4 %

ISO 527 | yield, 50 mm/min

Flexural modulus

23.0 °C

2.1 GPa

Show Supplier Material materials with Flexural modulus of 2.1 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

88 MPa

Show Supplier Material materials with Flexural strength of 88 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

60 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 60 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C

Impact strength, Izod notched

23.0 °C

65 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 65 kJ/m²

ISO 180/1A | 80*10*3, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

824 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 824 J/m

ASTM D 256

Instrumented Impact, Total Energy

23.0 °C

75 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 75 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

56 MPa

Show Supplier Material materials with Tensile strength of 56 MPa

ISO 527 | yield, 50 mm/min

Impact strength, Charpy unnotched

ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C

Impact strength, Izod unnotched

ISO 180/1U | unnotched 80*10*3, -30°C

Thermal

PropertyTemperatureValueComment

Ball Pressure Test

pass

IEC 60695-10-2 | 125°C +/- 2°C

Coefficient of thermal expansion

23.0 °C

6.7E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 6.7E-5 1/K

ISO 11359-2 | 23°C to 80°C

Coefficient of thermal expansion, transverse

23.0 °C

8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8E-5 1/K

ISO 11359-2 | 23°C to 80°C

Glow Wire Flammability Index

960 °C

Show Supplier Material materials with Glow Wire Flammability Index of 960 °C

Glow Wire Ignition Temperature

850 °C

Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C

IEC 60695-2-13 | 0.8 mm

Heat deflection temperature

118 °C

Show Supplier Material materials with Heat deflection temperature of 118 °C

Heat deflection temperature, 1.80 MPa

118 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 118 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

130 °C

Show Supplier Material materials with Relative temperature index, electrical of 130 °C

UL 746B

Relative temperature index, mechanical impact

120 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C

UL 746B

Relative temperature index, mechanical strength

130 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C

UL 746B

Vicat softening temperature

139 °C

Show Supplier Material materials with Vicat softening temperature of 139 °C

ISO 306 | Rate B/120

Flammability

UL Recognized, 94V-2 Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.0 mm: 875°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 0.8 mm: 825°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=256638- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

3 V

Show Supplier Material materials with Comparative tracking index of 3 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm

≥, UL 746A | PLC 1

Hot-Wire Ignition

23.0 °C

3 mm

Show Supplier Material materials with Hot-Wire Ignition of 3 mm

≥, UL 746A | PLC 2

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

10 g/10min

Show Supplier Material materials with Melt mass-flow rate of 10 g/10min

ASTM D 1238 | 300°C/1.2 kgf

Melt volume-flow rate

9 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 9 cm³/10min

ISO 1133 | MVR at 300°C/1.2 kg

Shrinkage

23.0 °C

0.4 %

Show Supplier Material materials with Shrinkage of 0.4 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Wireless Communications, Wearables, Personal Computing, Data Transfer, Cooking Range, Audio, Exercise Equipment, Heavy Vehicles, Enclosures

Availability

Europe,Asia,Americas

Processing methods

Shot to Cylinder Size: 40 to 60.0%
Drying Time (Cumulative): 48hrs
Back Pressure: 0.3 to 0.7MPa
Middle - Zone 2 Temperature: 280 to 305.0°C
Nozzle Temperature: 290 to 310.0°C
Drying Temperature: 120°C
Maximum Moisture Content: 0.02%
Drying Time: 3 to 4.0hrs
Rear - Zone 1 Temperature: 270 to 295.0°C
Front - Zone 3 Temperature: 295 to 315.0°C
Screw Speed: 40 to 70.0rpm
Melt Temperature: 295 to 315.0°C
Vent Depth: 0.025 to 0.076mm
Mold Temperature: 70 to 95.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.