Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.22 - 0.32 [-] Show Supplier Material materials with Coefficient of friction of 0.22 - 0.32 [-] | ||
Coefficient of friction, kinetic | 0.32 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.32 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.22 [-] Show Supplier Material materials with Coefficient of friction, static of 0.22 [-] | ASTM D 3702 Modified: Manual | |
Density | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Density of 1.17 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 5.6 % Show Supplier Material materials with Elongation of 5.6 % | ASTM D 638 | yield |
Flexural modulus | 23.0 °C | 1.9 GPa Show Supplier Material materials with Flexural modulus of 1.9 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 68 MPa Show Supplier Material materials with Flexural strength of 68 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 43 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 43 kJ/m² | ISO 180/1A | notched 80*10*4, -40°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 542 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 542 J/m | ASTM D 256 | -40°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1762 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1762 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 54 MPa Show Supplier Material materials with Tensile strength of 54 MPa | ASTM D 638 | break |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.01E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.01E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8.54E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8.54E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 120 °C Show Supplier Material materials with Heat deflection temperature of 120 °C | ||||
Heat deflection temperature, 1.80 MPa | 120 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 120 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283871- - <br> UL Recognized, 94HB Flame Class Rating: 1.2mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101283841- - |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Lab Ware and Clinical Diagnostics, Head Protection, Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |