General
Property | Temperature | Value | Comment |
---|---|---|---|
Limiting oxygen index | 23.0 °C | 24 % Show Supplier Material materials with Limiting oxygen index of 24 % | |
Relative density | 23.0 °C | 1.04 [-] Show Supplier Material materials with Relative density of 1.04 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Water absorption of 0.1 % | ASTM D 570 | (23°C/48hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 120 % Show Supplier Material materials with Elongation of 120 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 0.1 GPa Show Supplier Material materials with Flexural modulus of 0.1 GPa | ISO 178 | 12.5 mm/min |
Hardness, Shore A | 23.0 °C | 92 [-] Show Supplier Material materials with Hardness, Shore A of 92 [-] | ASTM D 2240 | 30S reading |
Tensile strength | 23.0 °C | 9 MPa Show Supplier Material materials with Tensile strength of 9 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | <, ASTM D 746 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 0 V Show Supplier Material materials with Comparative tracking index of 0 V | UL 746A | (UL) {PLC} |
Dielectric constant, 1MHz | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.8 [-] | IEC 60250 |
Dielectric strength | 23.0 °C | 23 kV/mm Show Supplier Material materials with Dielectric strength of 23 kV/mm | IEC 60243-1 | in oil, 2.0mm |
Dissipation factor, 1MHz | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 6E-3 [-] | IEC 60250 |
Volume resistivity | 23.0 °C | 4.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 4.00E+15 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 12 g/10min Show Supplier Material materials with Melt mass-flow rate of 12 g/10min | ASTM D 1238 | 210°C/5 kgf | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage, transverse of 0.4 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Shot to Cylinder Size: 30 to 70.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |