General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.69 g/cm³ Show Supplier Material materials with Density of 1.69 g/cm³ | ASTM D 792 |
Water absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Water absorption of 0.06 % | ISO 62-1 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 13 GPa Show Supplier Material materials with Elastic modulus of 13 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 0.8 % Show Supplier Material materials with Elongation of 0.8 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 12 GPa Show Supplier Material materials with Flexural modulus of 12 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 128 MPa Show Supplier Material materials with Flexural strength of 128 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 3 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 21 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 21 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 16 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 235 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 235 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 78 MPa Show Supplier Material materials with Tensile strength of 78 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 3.08E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.08E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 5.25E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5.25E-5 1/K | ASTM E 831 | 40°C to 120°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature | 162 - 204 °C Show Supplier Material materials with Heat deflection temperature of 162 - 204 °C | ||||
Heat deflection temperature, 0.45 MPa | 204 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 204 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 162 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 162 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 3.3 W/(m·K) Show Supplier Material materials with Thermal conductivity of 3.3 W/(m·K) | ISO 22007-2 | 60*60*3mm plaque | ||
Thermal conductivity, through-plane | 23.0 °C | 1 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 1 W/(m·K) | ISO 22007-2 | 60*60*3mm plaque | ||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101694795- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.8mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 800°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | IEC 60112 | |
Dielectric constant, 1GHz | 23.0 °C | 4.86 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 4.86 [-] | ASTM ES 7-83 | 1.1 GHz |
Dielectric strength | 23.0 °C | 10 kV/mm Show Supplier Material materials with Dielectric strength of 10 kV/mm | >, ASTM D 149 | in oil, 1.0 mm |
Dissipation factor, 1GHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 0.01 [-] | ASTM ES 7-83 | |
High Amp Arc Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with High Amp Arc Ignition of 0.8 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with Hot-Wire Ignition of 0.8 mm | ≥, UL 746A | PLC 1 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | LED Lighting, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |