General
Property | Temperature | Value | Comment |
---|---|---|---|
Water absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Water absorption of 0.06 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 9.5 % Show Supplier Material materials with Elongation of 9.5 % | ASTM D 638 | yld, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Flexural modulus of 2.6 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 111 MPa Show Supplier Material materials with Flexural strength of 111 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 160 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 160 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 55 MPa Show Supplier Material materials with Tensile strength of 55 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 122 - 133 °C Show Supplier Material materials with Heat deflection temperature of 122 - 133 °C | ||
Heat deflection temperature, 0.45 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 122 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C | ASTM D 648 | 6.4 mm, unannealed | |
Vicat softening temperature | 150 °C Show Supplier Material materials with Vicat softening temperature of 150 °C | ASTM D 1525 | Rate B/50 | |
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=237097- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1MHz | 23.0 °C | 2.49 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.49 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 2.57 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.57 [-] | ASTM D 150 | 50/60 Hz |
Dielectric strength | 23.0 °C | 18.8 kV/mm Show Supplier Material materials with Dielectric strength of 18.8 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Dissipation factor, 1MHz | 23.0 °C | 2.6E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2.6E-3 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 5.2E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 5.2E-3 [-] | ASTM D 150 | 50/60 Hz |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 2.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 2.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosures, Electronics, Energy Management, Enclosure/Housing/Cover, Heavy Vehicles, Head Protection, Gas/Electric Oven, Industrial Material Handling, Freezer, Auto Aftermarket, Circuit Protection, Air Conditioning, Dishwasher, Displays, Document Handling, Data Management, Bottles, Coffee Maker/Espresso Machine, Washing Machine, Vacuum Cleaner, Swimming Pool/Spa, Wireless Communications, Personal Care, Non-LED Lighting, Personal Computing, Laundry Dryer, Meter Water, LED Lighting, Photovoltaic Components, Power Manangement, Pump, Refrigerator, Small Appliance, Rail | |
Availability | Europe,Asia,Americas | |
Processing methods | Mold Temperature: 70 to 100.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |