General
Property | Temperature | Value | Comment |
---|---|---|---|
Water absorption | 23.0 °C | 0.2 % Show Supplier Material materials with Water absorption of 0.2 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 10 % Show Supplier Material materials with Elongation of 10 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Flexural modulus of 2.1 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 70 MPa Show Supplier Material materials with Flexural strength of 70 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 12 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 45 MPa Show Supplier Material materials with Tensile strength of 45 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 110 - 125 °C Show Supplier Material materials with Heat deflection temperature of 110 - 125 °C | ||
Heat deflection temperature, 0.45 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 125 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 110 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 110 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Vicat softening temperature | 130 °C Show Supplier Material materials with Vicat softening temperature of 130 °C | ISO 306 | Rate B/120 | |
Flammability | Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1MHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.6 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.7 [-] | IEC 60250 | 50/60 Hz |
Dielectric strength | 23.0 °C | 33 kV/mm Show Supplier Material materials with Dielectric strength of 33 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
Dissipation factor, 1MHz | 23.0 °C | 3E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 7E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 7E-3 [-] | IEC 60250 | 50/60 Hz |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosures, Electronics, Energy Management, Enclosure/Housing/Cover, Heavy Vehicles, Head Protection, Gas/Electric Oven, Industrial Material Handling, Freezer, Auto Aftermarket, Circuit Protection, Air Conditioning, Dishwasher, Displays, Document Handling, Data Management, Bottles, Coffee Maker/Espresso Machine, Washing Machine, Vacuum Cleaner, Swimming Pool/Spa, Wireless Communications, Personal Care, Non-LED Lighting, Personal Computing, Laundry Dryer, Meter Water, LED Lighting, Photovoltaic Components, Power Manangement, Pump, Refrigerator, Small Appliance, Rail | |
Availability | Europe,Asia,Americas | |
Processing methods | Mold Temperature: 90 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |