General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.24 [-] Show Supplier Material materials with Relative density of 1.24 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastic modulus of 2.6 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 67 % Show Supplier Material materials with Elongation of 67 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 112 MPa Show Supplier Material materials with Flexural strength of 112 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 181 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 181 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 181 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 181 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 74 MPa Show Supplier Material materials with Tensile strength of 74 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 30 g/10min Show Supplier Material materials with Melt mass-flow rate of 30 g/10min | ASTM D 1238 | 337°C/6.6 kgf | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage, transverse of 0.5 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures, Individual Equiptment, Head Protection, Data Transfer, Medical Device, Wireless Communications, Weapon | |
Availability | Americas | |
Processing methods | Vent Depth: 0.025 to 0.076mm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |