General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative density of 1.2 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2 GPa Show Supplier Material materials with Elastic modulus of 2 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 6 % Show Supplier Material materials with Elongation of 6 % | ASTM D 638 | yld, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 90 MPa Show Supplier Material materials with Flexural strength of 90 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 875 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 875 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 777 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 777 J/m | ASTM D 256 | notched, -30°C |
Tensile strength | 23.0 °C | 54 MPa Show Supplier Material materials with Tensile strength of 54 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 125 - 138 °C Show Supplier Material materials with Heat deflection temperature of 125 - 138 °C | ||
Heat deflection temperature, 0.45 MPa | 138 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 138 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ASTM D 648 | 3.2mm, unannealed | |
Vicat softening temperature | 143 °C Show Supplier Material materials with Vicat softening temperature of 143 °C | ASTM D 1525 | Rate B/50 | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104297933 - - <br> UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 10 g/10min Show Supplier Material materials with Melt mass-flow rate of 10 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 9.5 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 9.5 cm³/10min | ASTM D 1238 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | SABIC method |
Shrinkage, transverse | 23.0 °C | 0.6 % Show Supplier Material materials with Shrinkage, transverse of 0.6 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 3 to 4.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |