General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 38 % Show Supplier Material materials with Limiting oxygen index of 38 % | |
Relative density | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative density of 1.2 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 5.2 % Show Supplier Material materials with Elongation of 5.2 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Flexural modulus of 2.1 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 84 MPa Show Supplier Material materials with Flexural strength of 84 MPa | ISO 178 | yield, 2 mm/min |
Hardness, Rockwell L | 23.0 °C | 84 [-] Show Supplier Material materials with Hardness, Rockwell L of 84 [-] | ASTM D 785 |
Hardness, Rockwell R | 23.0 °C | 117 [-] Show Supplier Material materials with Hardness, Rockwell R of 117 [-] | ASTM D 785 |
Impact strength, Charpy notched | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 69 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C |
Impact strength, Izod notched | 23.0 °C | 73 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 73 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 700 J/m | ASTM D 256 | -40°C |
Instrumented Impact, Total Energy | 23.0 °C | 66 J Show Supplier Material materials with Instrumented Impact, Total Energy of 66 J | ASTM D 3763 | -30°C |
Tensile strength | 23.0 °C | 54 MPa Show Supplier Material materials with Tensile strength of 54 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.8E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 9.8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9.8E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature | 108 - 119 °C Show Supplier Material materials with Heat deflection temperature of 108 - 119 °C | ||||
Heat deflection temperature, 0.45 MPa | 119 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 119 °C | ISO 75/Cf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 108 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 108 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Vicat softening temperature | 124 °C Show Supplier Material materials with Vicat softening temperature of 124 °C | ISO 306 | Rate B/120 | |||
Flammability | Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥3.0mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104423704- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant | 23.0 °C | 2.81 [-] Show Supplier Material materials with Dielectric constant of 2.81 [-] | SABIC method | 1.9 GHz |
Dielectric constant, 10GHz | 23.0 °C | 2.84 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 2.84 [-] | SABIC method |
Dielectric constant, 1GHz | 23.0 °C | 2.87 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.87 [-] | SABIC method | 1.1 GHz |
Dielectric constant, 5GHz | 23.0 °C | 2.81 [-] Show Supplier Material materials with Dielectric constant, 5GHz of 2.81 [-] | SABIC method |
Dissipation factor | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor of 6E-3 [-] | SABIC method |
Dissipation factor, 1GHz | 23.0 °C | 6.4E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 6.4E-3 [-] | SABIC method | |
Dissipation factor, 5GHz | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor, 5GHz of 6E-3 [-] | SABIC method |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 12 g/10min Show Supplier Material materials with Melt mass-flow rate of 12 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 11 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 11 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage, transverse of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Building/Construction Sheet, Data Management, Data Transfer, Displays, Document Handling, Aerospace, Air Conditioning, Audio, Lawn/Garden, Heavy Vehicles, Freezer, Engine Cooling System, EV Infrastructure, Electronics, Energy Management, Enclosure/Housing/Cover, Enclosures, Electronic Components, Non-LED Lighting, Personal Computing, LED Lighting, Infrastructure, Small Appliance, Security/Detection, Respiratory, Photo/Video Camera, Vacuum Cleaner, Swimming Pool/Spa, Wiring Devices, Watch/Jewelry, Wearables, Wireless Communications, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |