General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 8 % Show Supplier Material materials with Elongation of 8 % | SABIC - Japan Method | break |
Flexural modulus | 23.0 °C | 5.6 GPa Show Supplier Material materials with Flexural modulus of 5.6 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 143 MPa Show Supplier Material materials with Flexural strength of 143 MPa | ASTM D 790 |
Hardness, Rockwell R | 23.0 °C | 127 [-] Show Supplier Material materials with Hardness, Rockwell R of 127 [-] | ASTM D 785 |
Impact strength, Izod notched | 23.0 °C | 87 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 87 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 87 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 87 J/m | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 107 MPa Show Supplier Material materials with Tensile strength of 107 MPa | SABIC - Japan Method | yield |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.7E-5 - 4.4E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.7E-5 - 4.4E-5 1/K | TMA | -30°C to 30°C |
Heat deflection temperature | 143 °C Show Supplier Material materials with Heat deflection temperature of 143 °C | ||
Heat deflection temperature, 1.80 MPa | 143 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 143 °C | ASTM D 648 | 6.4 mm, unannealed |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 19.8 g/10min Show Supplier Material materials with Melt mass-flow rate of 19.8 g/10min | ASTM D 1238 | 300°C/5.0 kgf | |
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Monitoring and Imaging, Personal Computing, Power Manangement, Pump, Electronic Components, Enclosure/Housing/Cover, Enclosures, EV Infrastructure, Document Handling, Data Transfer, Data Management, Air Conditioning | |
Availability | Asia | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |