General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 5.2 % Show Supplier Material materials with Elongation of 5.2 % | ISO 527 | yield |
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ISO 178 |
Flexural strength | 23.0 °C | 112 MPa Show Supplier Material materials with Flexural strength of 112 MPa | ISO 178 |
Hardness, Rockwell R | 23.0 °C | 119 [-] Show Supplier Material materials with Hardness, Rockwell R of 119 [-] | ASTM D 785 |
Impact strength, Izod notched | 23.0 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 15 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 55 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 55 J/m | ASTM D 256 | notched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 54 J Show Supplier Material materials with Instrumented Impact, Total Energy of 54 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 75 MPa Show Supplier Material materials with Tensile strength of 75 MPa | ISO 527 | yield |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature | 140 - 156 °C Show Supplier Material materials with Heat deflection temperature of 140 - 156 °C | ||||
Heat deflection temperature, 0.45 MPa | 156 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 156 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 140 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat softening temperature | 162 °C Show Supplier Material materials with Vicat softening temperature of 162 °C | ISO 306 | Rate B/50 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 825°C IEC 60695-2-13 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=627664- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 3 V Show Supplier Material materials with Comparative tracking index of 3 V | UL 746A | (UL) {PLC} |
Dielectric constant, 1MHz | 23.0 °C | 2.63 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.63 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 2.68 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.68 [-] | ASTM D 150 | 50/60 Hz |
Dielectric strength | 23.0 °C | 19.4 kV/mm Show Supplier Material materials with Dielectric strength of 19.4 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Dissipation factor, 1MHz | 23.0 °C | 9E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 9E-3 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 3.1E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 3.1E-3 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+17 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+17 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 7.4 g/10min Show Supplier Material materials with Melt mass-flow rate of 7.4 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Melt volume-flow rate | 7 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 7 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage, transverse of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Energy Management, Enclosure/Housing/Cover, Enclosures, Lawn/Garden, Heavy Vehicles, Gas/Electric Oven, Freezer, EV Infrastructure, Data Management, Document Handling, Displays, Amusement Machine, Circuit Protection, Personal Computing, Non-LED Lighting, Monitoring and Imaging, Medical Device, LED Lighting, Refrigerator, Power Manangement, Plumbing, Photovoltaic Components, Surgical Devices, Security/Detection, Washing Machine, Wireless Communications, Wiring Devices | |
Availability | Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |