General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Density of 1.31 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.35 % Show Supplier Material materials with Moisture absorption of 0.35 % | ISO 62 | (23°C / 50% RH) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 12.6 GPa Show Supplier Material materials with Elastic modulus of 12.6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 1.2 % Show Supplier Material materials with Elongation of 1.2 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 7.7 GPa Show Supplier Material materials with Flexural modulus of 7.7 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 216 MPa Show Supplier Material materials with Flexural strength of 216 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 53 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 28 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 28 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 448 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 448 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 11 J Show Supplier Material materials with Instrumented Impact, at Peak of 11 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 137 MPa Show Supplier Material materials with Tensile strength of 137 MPa | ISO 527 | break |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 3.3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.3E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 3.33E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 3.33E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 207 °C Show Supplier Material materials with Heat deflection temperature of 207 °C | ||||
Heat deflection temperature, 1.80 MPa | 207 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 207 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101345237- - <br> UL Recognized, 94V-0 Flame Class Rating: 0.35mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Transfer, Semiconductor | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |