General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Density of 1.31 g/cm³ | ISO 1183 | (Molded) |
Water absorption | 23.0 °C | 0.25 % Show Supplier Material materials with Water absorption of 0.25 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 9 GPa Show Supplier Material materials with Elastic modulus of 9 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.3 % Show Supplier Material materials with Elongation of 2.3 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 8.4 GPa Show Supplier Material materials with Flexural modulus of 8.4 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 225 MPa Show Supplier Material materials with Flexural strength of 225 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 3 kJ/m² | ISO 179/1eA | 80*10*4mm, Cut, 23°C |
Impact strength, Izod notched | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 32 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 32 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 32 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 156 MPa Show Supplier Material materials with Tensile strength of 156 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.56E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.56E-5 1/K | ASTM E 831 | 40°C to 120°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.25E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.25E-5 1/K | ASTM E 831 | 40°C to 120°C | ||
Heat deflection temperature | 201 °C Show Supplier Material materials with Heat deflection temperature of 201 °C | ||||
Heat deflection temperature, 1.80 MPa | 201 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 201 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101997197- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.4mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 397000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 397000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 508000 Ω·cm Show Supplier Material materials with Volume resistivity of 508000 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 31 g/10min Show Supplier Material materials with Melt mass-flow rate of 31 g/10min | ASTM D 1238 | 367°C/6.6 kgf | |
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage, transverse of 0.5 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |