LNP™ THERMOCOMP™ Compound EF006 - Europe

Want to keep this datasheet? Save it now in your required format

Description

LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber.

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.52 g/cm³

Show Supplier Material materials with Density of 1.52 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

10.4 GPa

Show Supplier Material materials with Elastic modulus of 10.4 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

2.2 %

Show Supplier Material materials with Elongation of 2.2 %

ISO 527 | break

Flexural modulus

23.0 °C

9.2 GPa

Show Supplier Material materials with Flexural modulus of 9.2 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

263 MPa

Show Supplier Material materials with Flexural strength of 263 MPa

ISO 178

Impact strength, Izod notched

23.0 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m²

ISO 180/1A | 80*10*4, 23°C

Impact strength, Izod unnotched

23.0 °C

45 kJ/m²

Show Supplier Material materials with Impact strength, Izod unnotched of 45 kJ/m²

ISO 180/1U | 80*10*4, 23°C

Tensile strength

23.0 °C

177 MPa

Show Supplier Material materials with Tensile strength of 177 MPa

ISO 527 | break

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

ISO 11359-2 | 23°C to 60°C

Coefficient of thermal expansion, transverse

23.0 °C

4.3E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 4.3E-5 1/K

ISO 11359-2 | 23°C to 60°C

Heat deflection temperature

209 °C

Show Supplier Material materials with Heat deflection temperature of 209 °C

Heat deflection temperature, 1.80 MPa

209 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 209 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

105 °C

Show Supplier Material materials with Relative temperature index, electrical of 105 °C

UL 746B

Relative temperature index, mechanical impact

105 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B

Relative temperature index, mechanical strength

105 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C

UL 746B

Flammability

UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101357465- -

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

SABIC method

Technological properties

Property
Application areas

Medical Device, Aircraft Exteriors, Aerospace

Availability

Europe,Americas

Processing methods

Drying Time: 4 to 6.0hrs
Mold Temperature: 140 to 180.0°C
Front - Zone 3 Temperature: 380 to 400.0°C
Maximum Moisture Content: 0.02%
Melt Temperature: 360 to 400.0°C
Back Pressure: 0.3 to 0.7MPa
Rear - Zone 1 Temperature: 360 to 380.0°C
Middle - Zone 2 Temperature: 370 to 390.0°C
Drying Temperature: 150°C
Nozzle Temperature: 390 to 400.0°C
Screw speed (Circumferential speed): 0.2 to 0.3m/s
Vent Depth: 0.025 to 0.076mm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.