General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Density of 1.33 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 1.6 % Show Supplier Material materials with Elongation of 1.6 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 11.7 GPa Show Supplier Material materials with Flexural modulus of 11.7 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 248 MPa Show Supplier Material materials with Flexural strength of 248 MPa | ASTM D 790 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 373 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 373 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 165 MPa Show Supplier Material materials with Tensile strength of 165 MPa | ASTM D 638 | break |
Thermal
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282750- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101345232- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 100 - 1000000 Ω·cm Show Supplier Material materials with Volume resistivity of 100 - 1000000 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management, Battery Cell, Auto Aftermarket | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |