General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.43 g/cm³ Show Supplier Material materials with Density of 1.43 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.11 % Show Supplier Material materials with Moisture absorption of 0.11 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Relative density | 23.0 °C | 1.44 [-] Show Supplier Material materials with Relative density of 1.44 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Compressive strength | 23.0 °C | 222 MPa Show Supplier Material materials with Compressive strength of 222 MPa | SABIC method |
Elastic modulus | 23.0 °C | 35.5 GPa Show Supplier Material materials with Elastic modulus of 35.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 0.9 % Show Supplier Material materials with Elongation of 0.9 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 30.6 GPa Show Supplier Material materials with Flexural modulus of 30.6 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 364 MPa Show Supplier Material materials with Flexural strength of 364 MPa | ISO 178 | break, 2 mm/min |
Hardness, Rockwell M | 23.0 °C | 112 [-] Show Supplier Material materials with Hardness, Rockwell M of 112 [-] | ASTM D 785 | |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 74 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 74 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 33 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 33 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 597 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 597 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 7 J Show Supplier Material materials with Instrumented Impact, Total Energy of 7 J | ASTM D 3763 | 23°C |
Poisson's ratio | 23.0 °C | 0.4 [-] Show Supplier Material materials with Poisson's ratio of 0.4 [-] | ASTM E 132 |
Shear modulus | 23.0 °C | 4.7 GPa Show Supplier Material materials with Shear modulus of 4.7 GPa | ASTM D732 |
Shear strength | 23.0 °C | 120 MPa Show Supplier Material materials with Shear strength of 120 MPa | ASTM D732 |
Tensile strength | 23.0 °C | 247 MPa Show Supplier Material materials with Tensile strength of 247 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.7E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.7E-6 1/K | ASTM E 831 | -40°C to 150°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 3.6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 3.6E-5 1/K | ASTM E 831 | -40°C to 150°C |
Heat deflection temperature | 193 °C Show Supplier Material materials with Heat deflection temperature of 193 °C | ||
Heat deflection temperature, 1.80 MPa | 193 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 193 °C | ASTM D 648 | 3.2mm, unannealed |
Electrical
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 15 g/10min Show Supplier Material materials with Melt mass-flow rate of 15 g/10min | ASTM D 1238 | 380°C/6.7 kgf | |
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage, transverse of 0.1 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Surgical Devices, Electronic Components, Enclosures, Aircraft Seating, Air Cabin Interiors, Building Accessory, Circuit Protection | |
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |