General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.39 [-] Show Supplier Material materials with Relative density of 1.39 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Compressive strength | 23.0 °C | 234 MPa Show Supplier Material materials with Compressive strength of 234 MPa | SABIC method |
Elastic modulus | 23.0 °C | 27.5 GPa Show Supplier Material materials with Elastic modulus of 27.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 1.4 % Show Supplier Material materials with Elongation of 1.4 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 23.3 GPa Show Supplier Material materials with Flexural modulus of 23.3 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 350 MPa Show Supplier Material materials with Flexural strength of 350 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 7 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 80 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 80 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 32 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 580 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 580 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 257 MPa Show Supplier Material materials with Tensile strength of 257 MPa | ISO 527 | break, 5 mm/min |
Thermal
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 10 g/10min Show Supplier Material materials with Melt mass-flow rate of 10 g/10min | ASTM D 1238 | 380°C/6.7 kgf | |
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | ASTM D 955 | 24 hrs |
Shrinkage, transverse | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage, transverse of 0.1 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Water Treatment/Filtration, Respiratory, Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |