General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Density of 1.38 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 20.2 GPa Show Supplier Material materials with Elastic modulus of 20.2 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 1.3 % Show Supplier Material materials with Elongation of 1.3 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 17.9 GPa Show Supplier Material materials with Flexural modulus of 17.9 GPa | ISO 178 |
Flexural strength | 23.0 °C | 269 MPa Show Supplier Material materials with Flexural strength of 269 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 35 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Tensile strength | 23.0 °C | 183 MPa Show Supplier Material materials with Tensile strength of 183 MPa | ISO 527 | break |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 217 °C Show Supplier Material materials with Heat deflection temperature of 217 °C | ||
Heat deflection temperature, 1.80 MPa | 217 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 217 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Flammability | UL Recognized, 94V-0 Flame Class Rating: 0.75mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344539- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Aircraft Exteriors, Air Cabin Interiors | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |