General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 19.1 GPa Show Supplier Material materials with Elastic modulus of 19.1 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 2.3 % Show Supplier Material materials with Elongation of 2.3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 15.8 GPa Show Supplier Material materials with Flexural modulus of 15.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 344 MPa Show Supplier Material materials with Flexural strength of 344 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 109 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 109 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 109 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 109 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 711 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 711 J/m | ASTM D 4812 | 23°C |
Poisson's ratio | 23.0 °C | 0.4 [-] Show Supplier Material materials with Poisson's ratio of 0.4 [-] | ASTM E 132 |
Shear modulus | 23.0 °C | 4.4 GPa Show Supplier Material materials with Shear modulus of 4.4 GPa | ASTM D732 |
Shear strength | 23.0 °C | 121.4 MPa Show Supplier Material materials with Shear strength of 121.4 MPa | ASTM D732 |
Tensile strength | 23.0 °C | 245 MPa Show Supplier Material materials with Tensile strength of 245 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.4E-6 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.4E-6 1/K | ISO 11359-2 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 5.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5.5E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Heat deflection temperature | 170 °C Show Supplier Material materials with Heat deflection temperature of 170 °C | ||
Heat deflection temperature, 1.80 MPa | 170 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 170 °C | ASTM D 648 | 3.2mm, unannealed |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100000 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100000 - 1000000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Aircraft Seating | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |