General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.17 [-] Show Supplier Material materials with Relative density of 1.17 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 1 % Show Supplier Material materials with Elongation of 1 % | Modified ASTM D638 | 5mm/min |
Flexural strength | 23.0 °C | 36 MPa Show Supplier Material materials with Flexural strength of 36 MPa | Modified ASTM D790 | 5mm/min |
Tensile strength | 23.0 °C | 75 MPa Show Supplier Material materials with Tensile strength of 75 MPa | Modified ASTM D638 | 5mm/min |
Thermal
Technological properties
Property | ||
---|---|---|
Application areas | Additive Plastic | |
Availability | Europe,Asia,Americas | |
Processing methods | Extruder L/D: 24- | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |