Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.29 g/cm³ Show Supplier Material materials with Density of 1.29 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.8 GPa Show Supplier Material materials with Elastic modulus of 2.8 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 4 - 8 % Show Supplier Material materials with Elongation of 4 - 8 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 2.6 GPa Show Supplier Material materials with Flexural modulus of 2.6 GPa | ISO 178 |
Flexural strength | 23.0 °C | 80 MPa Show Supplier Material materials with Flexural strength of 80 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 11 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 122 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 122 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 85 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1788 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1788 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 57 MPa Show Supplier Material materials with Tensile strength of 57 MPa | ISO 527 | yield |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5.6E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.6E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 125 - 136 °C Show Supplier Material materials with Heat deflection temperature of 125 - 136 °C | ||||
Heat deflection temperature, 0.45 MPa | 136 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 136 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | UL 746B | |||
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101343783- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101343784- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.6mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000 Ω | ASTM D 257 |
Shielding effectiveness | 23.0 °C | 40 dB Show Supplier Material materials with Shielding effectiveness of 40 dB | SABIC method | @ 3mm |
Volume resistivity | 23.0 °C | 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 10000 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Personal Computing, Power Manangement, Enclosures, Electronic Components, Lab Ware and Clinical Diagnostics, Individual Equiptment, Data Transfer, Conveyor | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |