LNP LUBRICOMP MFL36S is a compound based on Polypropylene resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.27 g/cm³

Show Supplier Material materials with Density of 1.27 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

7.6 GPa

Show Supplier Material materials with Elastic modulus of 7.6 GPa

ASTM D 638 | 50 mm/min

Elongation

23.0 °C

2.9 %

Show Supplier Material materials with Elongation of 2.9 %

ASTM D 638 | break

Flexural modulus

23.0 °C

5.9 GPa

Show Supplier Material materials with Flexural modulus of 5.9 GPa

ASTM D 790

Flexural strength

23.0 °C

117 MPa

Show Supplier Material materials with Flexural strength of 117 MPa

ASTM D 790

Impact strength, Izod notched

23.0 °C

90 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 90 kJ/m²

ASTM D 256 | notched, 23°C

Tensile strength

23.0 °C

71 MPa

Show Supplier Material materials with Tensile strength of 71 MPa

ASTM D 638 | break

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.4 %

Show Supplier Material materials with Shrinkage of 0.4 %

ASTM D 955 | 24 hrs

Technological properties

Property
Application areas

Industrial Material Handling, Engine Component, Engine Cooling System, Electronic Components, Enclosures, Enclosure/Housing/Cover, Cooking Range, Auto Aftermarket, Non-LED Lighting

Availability

Europe,Asia,Americas

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.