LEXAN™ Copolymer LUX9130C - Americas

Want to keep this datasheet? Save it now in your required format

Description

Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and is UV stabilized providing additional weathering capability. Lexan* LUX9130C is available in clear transparent and tinted color options that is an excellent candidate for a wide variety of applications.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.11 %

Show Supplier Material materials with Moisture absorption of 0.11 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.19 [-]

Show Supplier Material materials with Relative density of 1.19 [-]

ASTM D 792

Water absorption

23.0 °C

0.13 %

Show Supplier Material materials with Water absorption of 0.13 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.3 GPa

Show Supplier Material materials with Elastic modulus of 2.3 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

73 %

Show Supplier Material materials with Elongation of 73 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

2.4 GPa

Show Supplier Material materials with Flexural modulus of 2.4 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

96 MPa

Show Supplier Material materials with Flexural strength of 96 MPa

ISO 178 | yield, 2 mm/min

Hardness, Ball Indentation

23.0 °C

138 MPa

Show Supplier Material materials with Hardness, Ball Indentation of 138 MPa

ISO 2039-1 | H358/30

Impact strength, Charpy notched

23.0 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C

Impact strength, Izod notched

23.0 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m²

ISO 180/1A | 80*10*3, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

100 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m

ASTM D 256

Instrumented Impact, Total Energy

23.0 °C

65 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 65 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

63 MPa

Show Supplier Material materials with Tensile strength of 63 MPa

ISO 527 | yield, 50 mm/min

Impact strength, Charpy unnotched

ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C

Impact strength, Izod unnotched

ISO 180/1U | unnotched 80*10*3, -30°C

Impact strength, Izod unnotched, ASTM

ASTM D 4812 | 23°C

Thermal

PropertyTemperatureValueComment

Ball Pressure Test

Pass

IEC 60695-10-2 | 125°C +/- 2°C

Coefficient of thermal expansion

23.0 °C

7.7E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7.7E-5 1/K

ISO 11359-2 | 23°C to 80°C

Coefficient of thermal expansion, transverse

23.0 °C

8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8E-5 1/K

ISO 11359-2 | 23°C to 80°C

Glow Wire Flammability Index

960 °C

Show Supplier Material materials with Glow Wire Flammability Index of 960 °C

Glow Wire Ignition Temperature

850 °C

Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C

IEC 60695-2-13 | 3.0 mm

Heat deflection temperature

121 - 131 °C

Show Supplier Material materials with Heat deflection temperature of 121 - 131 °C

Heat deflection temperature, 0.45 MPa

131 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 131 °C

ISO 75/Be | Edgew 120*10*4 sp=100mm

Heat deflection temperature, 1.80 MPa

121 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 121 °C

ISO 75/Ae | Edgew 120*10*4 sp=100mm

Relative temperature index, electrical

130 °C

Show Supplier Material materials with Relative temperature index, electrical of 130 °C

UL 746B

Relative temperature index, mechanical impact

120 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C

UL 746B

Relative temperature index, mechanical strength

130 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C

UL 746B

Vicat softening temperature

146 °C

Show Supplier Material materials with Vicat softening temperature of 146 °C

ISO 306 | Rate A/50

Flammability

UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 850°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F1- UL 746C <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101088457- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

3 V

Show Supplier Material materials with Comparative tracking index of 3 V

UL 746A | (UL) {PLC}

Dielectric constant, 1GHz

23.0 °C

2.78 [-]

Show Supplier Material materials with Dielectric constant, 1GHz of 2.78 [-]

ASTM ES 7-83 | 1.1 GHz

Dielectric constant, 1MHz

23.0 °C

2.7 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.7 [-]

IEC 62631-2-1

Dielectric constant, 60Hz

23.0 °C

2.4 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.4 [-]

IEC 62631-2-1 | 50/60 Hz

Dielectric strength

23.0 °C

18 kV/mm

Show Supplier Material materials with Dielectric strength of 18 kV/mm

IEC 60243-1 | in oil, 3.2 mm,

Dissipation factor, 1GHz

23.0 °C

5.6E-3 [-]

Show Supplier Material materials with Dissipation factor, 1GHz of 5.6E-3 [-]

ASTM ES 7-83 |

Dissipation factor, 1MHz

23.0 °C

0.01 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-]

IEC 62631-2-1

Dissipation factor, 50Hz

23.0 °C

1E-3 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 1E-3 [-]

IEC 62631-2-1 | 50/60 Hz

High Amp Arc Ignition

23.0 °C

0.4 mm

Show Supplier Material materials with High Amp Arc Ignition of 0.4 mm

≥, UL 746A | PLC 1

Hot-Wire Ignition

23.0 °C

0.4 mm

Show Supplier Material materials with Hot-Wire Ignition of 0.4 mm

≥, UL 746A | PLC 3

Sheet resistivity, ROA

23.0 °C

1.00E+16 - 1.00E+17 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 - 1.00E+17 Ω

IEC 62631-3-2

Volume resistivity

23.0 °C

1.00E+16 - 1.00E+17 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+16 - 1.00E+17 Ω·cm

IEC 62631-3-1

Optical

PropertyValueComment

Transmission

91 %

Show Supplier Material materials with Transmission of 91 %

>, ASTM D 1003 | 2.54 mm

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

18 g/10min

Show Supplier Material materials with Melt mass-flow rate of 18 g/10min

ASTM D 1238 | 300°C/1.2 kgf

Melt volume-flow rate

17 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 17 cm³/10min

ISO 1133 | MVR at 300°C/1.2 kg

Shrinkage

23.0 °C

0.55 %

Show Supplier Material materials with Shrinkage of 0.55 %

SABIC method | 3.2 mm

Shrinkage, transverse

23.0 °C

0.6 %

Show Supplier Material materials with Shrinkage, transverse of 0.6 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

LED Lighting, Non-LED Lighting

Availability

Europe,Asia,Americas

Processing methods

Screw Speed: 40 to 70.0rpm
Rear - Zone 1 Temperature: 260 to 280.0°C
Nozzle Temperature: 275 to 300.0°C
Mold Temperature: 70 to 95.0°C
Shot to Cylinder Size: 40 to 60.0%
Drying Time (Cumulative): 48hrs
Drying Temperature: 120°C
Melt Temperature: 280 to 305.0°C
Drying Time: 3 to 4.0hrs
Back Pressure: 0.3 to 0.7MPa
Front - Zone 3 Temperature: 280 to 305.0°C
Vent Depth: 0.025 to 0.076mm
Middle - Zone 2 Temperature: 270 to 295.0°C
Maximum Moisture Content: 0.02%

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.