General
Property | Temperature | Value | Comment |
---|---|---|---|
Water absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Water absorption of 0.06 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 30 % Show Supplier Material materials with Elongation of 30 % | ASTM D 638 | brk, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 93 MPa Show Supplier Material materials with Flexural strength of 93 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 208 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 208 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 58 MPa Show Supplier Material materials with Tensile strength of 58 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.3E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.3E-4 1/K | ASTM E 831 | -40°C to 60°C | ||
Heat deflection temperature | 117 °C Show Supplier Material materials with Heat deflection temperature of 117 °C | ||||
Heat deflection temperature, 1.80 MPa | 117 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 117 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 90 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Flammability | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228540- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 2 V Show Supplier Material materials with Comparative tracking index of 2 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 1 |
Technological properties
Property | ||
---|---|---|
Application areas | Meter Water, Meter Gas, Medical Device, Personal Care, Personal Computing, Pump, Pipe/Fitting, Refrigerator, Plumbing, Small Appliance, Servingware, Seating/Chair, Surgical Devices, Water Treatment/Filtration, Watch/Jewelry, Wiring Devices, Wireless Communications, Vacuum Cleaner, Hot Water System, Fixture Bath/Shower, Food Processor, Electronic Components, Enclosures, Document Handling, Displays, Dishwasher, Coffee Maker/Espresso Machine, Commercial Storage/Cookware, Cooking Range, Aerospace, Animal Testing, Building Accessory, Irrigation | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 280 to 310.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |