General
Property | Temperature | Value | Comment |
---|---|---|---|
Relative density | 23.0 °C | 1.34 [-] Show Supplier Material materials with Relative density of 1.34 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 4.2 % Show Supplier Material materials with Elongation of 4.2 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 5.3 GPa Show Supplier Material materials with Flexural modulus of 5.3 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 101 MPa Show Supplier Material materials with Flexural strength of 101 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 74 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 74 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 74 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 74 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 357 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 357 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 16 J Show Supplier Material materials with Instrumented Impact, Total Energy of 16 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 74 MPa Show Supplier Material materials with Tensile strength of 74 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 99 - 105 °C Show Supplier Material materials with Heat deflection temperature of 99 - 105 °C | ||
Heat deflection temperature, 0.45 MPa | 105 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 105 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 99 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 99 °C | ASTM D 648 | 6.4 mm, unannealed | |
Flammability | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=228536- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,MEA,Americas,Global | |
Processing methods | Drying Temperature: 105 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |