General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.11 g/cm³ Show Supplier Material materials with Density of 1.11 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.8 GPa Show Supplier Material materials with Elastic modulus of 2.8 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 9 % Show Supplier Material materials with Elongation of 9 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 2.8 GPa Show Supplier Material materials with Flexural modulus of 2.8 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 115 MPa Show Supplier Material materials with Flexural strength of 115 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 40 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 40 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 50 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 600 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 600 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 55 MPa Show Supplier Material materials with Tensile strength of 55 MPa | ISO 527 | break, 50 mm/min |
Thermal
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant | 23.0 °C | 2.65 [-] Show Supplier Material materials with Dielectric constant of 2.65 [-] | SABIC method | 1.9 GHz |
Dielectric constant, 10GHz | 23.0 °C | 2.65 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 2.65 [-] | SABIC method |
Dielectric constant, 1GHz | 23.0 °C | 2.65 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.65 [-] | SABIC method | 1.1 GHz |
Dissipation factor | 23.0 °C | 1.4E-3 [-] Show Supplier Material materials with Dissipation factor of 1.4E-3 [-] | SABIC method |
Dissipation factor, 1GHz | 23.0 °C | 1.2E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 1.2E-3 [-] | SABIC method | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical Components & Infrastructure | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |