LNP™ THERMOCOMP™ Compound UF0067V

Want to keep this datasheet? Save it now in your required format

Description

LNP THERMOCOMP UF0067V is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring) applications. Additional feature is high heat such that articles made of it can survive SMT process.

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Relative density

23.0 °C

1.45 [-]

Show Supplier Material materials with Relative density of 1.45 [-]

ASTM D 792

Water absorption

23.0 °C

0.05 %

Show Supplier Material materials with Water absorption of 0.05 %

ISO 62-1 | (23°C/24hrs)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

9.5 GPa

Show Supplier Material materials with Elastic modulus of 9.5 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

1.6 %

Show Supplier Material materials with Elongation of 1.6 %

ASTM D 638 | brk, Type I, 5 mm/min

Flexural modulus

23.0 °C

8.5 GPa

Show Supplier Material materials with Flexural modulus of 8.5 GPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural strength

23.0 °C

150 MPa

Show Supplier Material materials with Flexural strength of 150 MPa

ASTM D 790 | yld, 1.3 mm/min, 50 mm span

Impact strength, Izod notched

23.0 °C

34 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 34 kJ/m²

ASTM D 256 | notched, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

34 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 34 J/m

ASTM D 256 | notched, 23°C

Impact strength, Izod unnotched, ASTM

23.0 °C

300 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 300 J/m

ASTM D 4812 | 23°C

Tensile strength

23.0 °C

104 MPa

Show Supplier Material materials with Tensile strength of 104 MPa

ASTM D 638 | brk, Type I, 5 mm/min

Thermal

PropertyValueComment

Heat deflection temperature

255 - 276 °C

Show Supplier Material materials with Heat deflection temperature of 255 - 276 °C

Heat deflection temperature, 0.45 MPa

276 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 276 °C

ASTM D 648 | 3.2 mm

Heat deflection temperature, 1.80 MPa

255 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 255 °C

ASTM D 648 | 1.82 MPa, 3.2 mm

Relative temperature index, electrical

65 °C

Show Supplier Material materials with Relative temperature index, electrical of 65 °C

UL 746B

Relative temperature index, mechanical impact

65 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C

UL 746B

Relative temperature index, mechanical strength

65 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C

UL 746B

Flammability

UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103351790- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.4mm UL 94

Electrical

PropertyTemperatureValueComment

Dielectric constant, 1GHz

23.0 °C

3.56 [-]

Show Supplier Material materials with Dielectric constant, 1GHz of 3.56 [-]

SABIC method | 1.1 GHz

Dissipation factor, 1GHz

23.0 °C

9E-3 [-]

Show Supplier Material materials with Dissipation factor, 1GHz of 9E-3 [-]

SABIC method |

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

SABIC method

Shrinkage, transverse

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage, transverse of 0.5 %

SABIC method

Technological properties

Property
Application areas

Antenna

Availability

Europe,Asia,Americas

Processing methods

Drying Temperature: 120°C
Drying Time: 4 to 7.0hrs
Melt Temperature: 290 to 330.0°C
Nozzle Temperature: 300 to 320.0°C
Front - Zone 3 Temperature: 300 to 320.0°C
Middle - Zone 2 Temperature: 280 to 300.0°C
Rear - Zone 1 Temperature: 260 to 280.0°C
Mold Temperature: 120 to 150.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.